General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 771.1 Kg Show Supplier Material materials with Bonding strength of 771.1 Kg | ASTM D229 | Condition A |
Densidad | 1.44 g/cm³ Show Supplier Material materials with Densidad of 1.44 g/cm³ | ASTM D792 | |
Moisture absorption | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | ASTM D570 | Condition A |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 105 [-] Show Supplier Material materials with Dureza Rockwell M of 105 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 64 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 64 J/m | ASTM D256 | Condition E-48/50, Transverse |
107 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 107 J/m | ASTM D256 | Condition E-48/50 | |
Resistencia a la compresión | 262 MPa Show Supplier Material materials with Resistencia a la compresión of 262 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 124.1 MPa Show Supplier Material materials with Resistencia a la flexión of 124.1 MPa | ASTM D790 | Condition A |
Resistencia a la tracción | 82.7 MPa Show Supplier Material materials with Resistencia a la tracción of 82.7 MPa | ASTM D638 | Condition A |
Resistencia al cizallamiento | 89.6 MPa Show Supplier Material materials with Resistencia al cizallamiento of 89.6 MPa | ASTM D732 | Condition A, Transverse |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL Bulletin 746b¹ | |
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications includepintle and stave-type bearings for rudder shafts in the marine industry. This material is known industry wide as “Marine Micarta.” This product is also suitable for heavy equipment applications that require finer machining profiles than those provided by bearing-grade laminates. | |
Fillers | Cotton Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |