Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 907.2 Kg Show Supplier Material materials with Bonding strength of 907.2 Kg | ASTM D229 | Condition A |
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | ASTM D792 | |
Moisture absorption | 0.08 % Show Supplier Material materials with Moisture absorption of 0.08 % | ASTM D570 | Condition A |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 80 [-] Show Supplier Material materials with Dureza Rockwell M of 80 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 154 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 154 J/m | ASTM D256 | Condition E-48/50, Transverse |
320 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 320 J/m | ASTM D256 | Condition E-48/50 | |
Módulo de flexión | 5.6 GPa Show Supplier Material materials with Módulo de flexión of 5.6 GPa | ASTM D790 | Condition A, Transverse |
6.5 GPa Show Supplier Material materials with Módulo de flexión of 6.5 GPa | ASTM D790 | Condition A | |
Resistencia a la compresión | 234.4 MPa Show Supplier Material materials with Resistencia a la compresión of 234.4 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 87.6 MPa Show Supplier Material materials with Resistencia a la flexión of 87.6 MPa | ASTM D790 | Condition A, Transverse |
111.7 MPa Show Supplier Material materials with Resistencia a la flexión of 111.7 MPa | ASTM D790 | Condition A | |
Resistencia a la tracción | 70.3 MPa Show Supplier Material materials with Resistencia a la tracción of 70.3 MPa | ASTM D638 | Condition A |
Resistencia al cizallamiento | 84.1 MPa Show Supplier Material materials with Resistencia al cizallamiento of 84.1 MPa | ASTM D732 | Condition A, Transverse |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.64e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.64e-05 1/K | IPC-TM 650-2.4.24 | |||
3.94e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.94e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL Bulletin 746b¹ | |||
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | BP18NPM is specifically designed for highly loaded bearing applications, where the lubrication is provided by the molybdenum disulfide. It may have a slightly greenish tint in the finished laminate. | |
Fillers | Cotton Fabric and MoS2 | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |