General
Property | Value | Comment |
---|---|---|
Bonding strength | 567 Kg Show Supplier Material materials with Bonding strength of 567 Kg | Condition A |
621 Kg Show Supplier Material materials with Bonding strength of 621 Kg | Condition D-48/50 | |
Moisture absorption | 1.19 % Show Supplier Material materials with Moisture absorption of 1.19 % | Condition D₁-24/23 |
Mecánica
Property | Value | Comment |
---|---|---|
Impact strength, Izod unnotched, ASTM | 77.9 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 77.9 J/m | Condition E-48/50, Transverse |
104.6 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 104.6 J/m | Condition E-48/50 | |
Resistencia a la flexión | 148.2 MPa Show Supplier Material materials with Resistencia a la flexión of 148.2 MPa | Condition A, Transverse |
151.7 MPa Show Supplier Material materials with Resistencia a la flexión of 151.7 MPa | Condition A |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Eléctrico
Property | Value | Comment |
---|---|---|
Tensión de ruptura | 25 kV Show Supplier Material materials with Tensión de ruptura of 25 kV | ondition A |
Technological properties
Property | ||
---|---|---|
Fillers | Cotton Fabric and PTFE | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |