General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 1088.6 Kg Show Supplier Material materials with Bonding strength of 1088.6 Kg | ASTM D229 | Condition A |
Densidad | 1.54 g/cm³ Show Supplier Material materials with Densidad of 1.54 g/cm³ | ASTM D792 | |
Moisture absorption | 1.94 % Show Supplier Material materials with Moisture absorption of 1.94 % | ASTM D570 | Condition D₁-24/23 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 95 [-] Show Supplier Material materials with Dureza Rockwell M of 95 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 390 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 390 J/m | ASTM D256 | Condition E-48/50, Transverse |
1222 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1222 J/m | ASTM D256 | Condition E-48/50 | |
Resistencia a la compresión | 280.6 MPa Show Supplier Material materials with Resistencia a la compresión of 280.6 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 106.9 MPa Show Supplier Material materials with Resistencia a la flexión of 106.9 MPa | ASTM D790 | Condition E-1/150, Transverse |
120.7 MPa Show Supplier Material materials with Resistencia a la flexión of 120.7 MPa | ASTM D790 | Condition A, Transverse | |
201.3 MPa Show Supplier Material materials with Resistencia a la flexión of 201.3 MPa | ASTM D790 | Condition E-1/150 | |
253 MPa Show Supplier Material materials with Resistencia a la flexión of 253 MPa | ASTM D790 | Condition A | |
Resistencia a la tracción | 176.5 MPa Show Supplier Material materials with Resistencia a la tracción of 176.5 MPa | ASTM D638 | Condition A |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.7e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.7e-05 1/K | IPC-TM 650-2.4.24 | |||
3.98e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.98e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, mechanical strength | 165 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 165 °C | UL Bulletin 746b¹ | |||
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | Applications include wear plates for conveyor systems, valve plates, and compressor and pump vanes | |
Fillers | Cotton Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |