General
Property | Value | Comment |
---|---|---|
Bonding strength | 408.2 Kg Show Supplier Material materials with Bonding strength of 408.2 Kg | |
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | |
Moisture absorption | 0.37 - 0.6 % Show Supplier Material materials with Moisture absorption of 0.37 - 0.6 % | Condition D₁-24/23 | Depending on the thickness of the specimen |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Rockwell M | 115 [-] Show Supplier Material materials with Dureza Rockwell M of 115 [-] | |
Impact strength, Izod unnotched, ASTM | 29.9 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 29.9 J/m | Transverse |
34.7 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 34.7 J/m | ||
Resistencia a la compresión | 304.1 MPa Show Supplier Material materials with Resistencia a la compresión of 304.1 MPa | Flatwise |
Resistencia a la flexión | 191.0 MPa Show Supplier Material materials with Resistencia a la flexión of 191.0 MPa | |
193.1 MPa Show Supplier Material materials with Resistencia a la flexión of 193.1 MPa | Transverse | |
Resistencia a la tracción | 116.5 MPa Show Supplier Material materials with Resistencia a la tracción of 116.5 MPa |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | ¹ | |
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | ¹ | |
Temperatura de transición del vidrio | 130 °C Show Supplier Material materials with Temperatura de transición del vidrio of 130 °C | min. | DSC | |
145 °C Show Supplier Material materials with Temperatura de transición del vidrio of 145 °C | max. | DMA | ||
Arc resistance | 120 seconds | ||
Inflamabilidad | UL 94, Class HB |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
6.6 [-] Show Supplier Material materials with Constante dieléctrica of 6.6 [-] | 1MHz | ASTM D150 | Condition A | |
Factor de disipación | 0.054 [-] Show Supplier Material materials with Factor de disipación of 0.054 [-] | 1MHz | Condition A | |
0.057 [-] Show Supplier Material materials with Factor de disipación of 0.057 [-] | 1MHz | Condition D-24/23 | ||
Rigidez dieléctrica | 6.69 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 6.69 kV/mm | |||
Tensión de ruptura | 6 kV Show Supplier Material materials with Tensión de ruptura of 6 kV | ASTM D149 | Condition D48/50 | |
65 kV Show Supplier Material materials with Tensión de ruptura of 65 kV | ASTM D149 | Condition A | ||
Índice de seguimiento comparativo | 150 V Show Supplier Material materials with Índice de seguimiento comparativo of 150 V |
Technological properties
Property | ||
---|---|---|
Application areas | It is designed to be used in tap changers, coil support plates and terminal panels for transformers and their accessories. | |
Fillers | Paper | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |