General
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 90 [-] Show Supplier Material materials with Dureza Rockwell M of 90 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 27 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 27 J/m | ASTM D256 | Condition E-48/50, Transverse |
29 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 29 J/m | ASTM D256 | Condition E-48/50 | |
Resistencia a la compresión | 241.3 MPa Show Supplier Material materials with Resistencia a la compresión of 241.3 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 172.4 MPa Show Supplier Material materials with Resistencia a la flexión of 172.4 MPa | ASTM D790 | Condition A |
172.4 MPa Show Supplier Material materials with Resistencia a la flexión of 172.4 MPa | ASTM D790 | Condition A, Transverse | |
Resistencia a la tracción | 117.2 MPa Show Supplier Material materials with Resistencia a la tracción of 117.2 MPa | ASTM D638 | Condition A |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL Bulletin 746b¹ | |
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | This material is normally used in the printed circuit board industry as a backup for the drilling operation. However, it is also used in other industries for tooling stock because of its ease of machining and good dimensional stability. | |
Fillers | Paper | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |