General
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 108 [-] Show Supplier Material materials with Dureza Rockwell M of 108 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 120 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 120 J/m | ASTM D256 | Condition E-48/50, Transverse |
178 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 178 J/m | ASTM D256 | Condition E-48/50 | |
Módulo de flexión | 10.3 GPa Show Supplier Material materials with Módulo de flexión of 10.3 GPa | ASTM D790 | Condition A, Transverse |
12.4 GPa Show Supplier Material materials with Módulo de flexión of 12.4 GPa | ASTM D790 | Condition A | |
Resistencia a la compresión | 286.1 MPa Show Supplier Material materials with Resistencia a la compresión of 286.1 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 307.5 MPa Show Supplier Material materials with Resistencia a la flexión of 307.5 MPa | ASTM D790 | Condition A, Transverse |
355.8 MPa Show Supplier Material materials with Resistencia a la flexión of 355.8 MPa | ASTM D790 | Condition A | |
Resistencia a la tracción | 164.8 MPa Show Supplier Material materials with Resistencia a la tracción of 164.8 MPa | ASTM D638 | Condition A |
Resistencia al cizallamiento | 96.5 MPa Show Supplier Material materials with Resistencia al cizallamiento of 96.5 MPa | ASTM D732 | Condition A, Transverse |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.3e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.3e-05 1/K | IPC-TM 650-2.4.24 | |||
1.5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL Bulletin 746b¹ | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL Bulletin 746b¹ | |||
Arc resistance | 120 seconds, ASTM D495, Condition A | ||||
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 5.2 [-] Show Supplier Material materials with Constante dieléctrica of 5.2 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
Factor de disipación | 0.037 [-] Show Supplier Material materials with Factor de disipación of 0.037 [-] | 1MHz | ASTM D150 | Condition D-24/23 |
Rigidez dieléctrica | 21.65 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 21.65 kV/mm | ASTM D149 | Condition D-48/50 | |
23.62 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 23.62 kV/mm | ASTM D149 | Condition A | ||
Tensión de ruptura | 7 kV Show Supplier Material materials with Tensión de ruptura of 7 kV | ASTM D149 | Condition D48/50 | |
53 kV Show Supplier Material materials with Tensión de ruptura of 53 kV | ASTM D149 | Condition A | ||
Índice de seguimiento comparativo | 200 V Show Supplier Material materials with Índice de seguimiento comparativo of 200 V | ASTM D3638 |
Technological properties
Property | ||
---|---|---|
Fillers | Paper | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |