General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 340.2 Kg Show Supplier Material materials with Bonding strength of 340.2 Kg | ASTM D229 | Condition A |
Densidad | 1.88 g/cm³ Show Supplier Material materials with Densidad of 1.88 g/cm³ | ASTM D792 | |
Moisture absorption | 0.19 % Show Supplier Material materials with Moisture absorption of 0.19 % | ASTM D570 | Condition D₁-24/23 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 100 [-] Show Supplier Material materials with Dureza Rockwell M of 100 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 614 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 614 J/m | ASTM D256 | Condition E-48/50, Transverse |
907 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 907 J/m | ASTM D256 | Condition E-48/50 | |
Resistencia a la flexión | 149.6 MPa Show Supplier Material materials with Resistencia a la flexión of 149.6 MPa | ASTM D790 | Condition A, Transverse |
167.5 MPa Show Supplier Material materials with Resistencia a la flexión of 167.5 MPa | ASTM D790 | Condition A |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL Bulletin 746b¹ | |
Relative temperature index, mechanical strength | 220 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 220 °C | UL Bulletin 746b¹ | |
Arc resistance | 200 seconds, ASTM D495, Condition A | ||
Inflamabilidad | UL Bulletin 94, Class V-0, Condition A |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.55 [-] Show Supplier Material materials with Constante dieléctrica of 4.55 [-] | 1MHz | ASTM D150 | Condition A |
4.67 [-] Show Supplier Material materials with Constante dieléctrica of 4.67 [-] | 1MHz | ASTM D150 | Condition D-24/23 | |
Factor de disipación | 0.018 [-] Show Supplier Material materials with Factor de disipación of 0.018 [-] | 1MHz | Condition A | |
0.045 [-] Show Supplier Material materials with Factor de disipación of 0.045 [-] | 1MHz | Condition D-24/23 | ||
Rigidez dieléctrica | 13.78 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 13.78 kV/mm | ASTM D149 | Condition A | |
Tensión de ruptura | 32 kV Show Supplier Material materials with Tensión de ruptura of 32 kV | ASTM D149 | Condition D48/50 | |
55 kV Show Supplier Material materials with Tensión de ruptura of 55 kV | ASTM D149 | Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | It can be substituted for NEMA G-7, in most heating, appliance insulation and some bearing applications. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |