General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 1.24 g/cm³ Show Supplier Material materials with Densidad of 1.24 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 140 % Show Supplier Material materials with Elongación of 140 % | ASTM D638 |
Flexural yield strength | 20.0 °C | 90 MPa Show Supplier Material materials with Flexural yield strength of 90 MPa | ASTM D790 |
Impact strength, Izod notched, ASTM | 20.0 °C | 24 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 24 J/m | ASTM D256 |
Módulo de flexión | 20.0 °C | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | ASTM D790 |
Aplicaciones térmicas
Óptico
Technological properties
Property | ||
---|---|---|
Application areas | Food packaging containers, blow molding, sheets and films,durables injection molding articles | |
Compliance | Akestra™ and/or its monomers are approved as food contact material in Europe (EFSA) and USA (FDA). Akestra™ complies with RoHS. All raw materials are REACH registered. A document of compliance is available on request with details about its regulatory and compliances. | |
Processing methods | Desiccant dryer and/or vented extrusion equipment. More information are available on request, TI-1800 and TI-1801 |