General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.83 - 0.89 g/cm³ Show Supplier Material materials with Densidad of 0.83 - 0.89 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 5 - 11 [-] Show Supplier Material materials with Dureza Shore A of 5 - 11 [-] | ASTM D2240 | |
Elongación | 1100 % Show Supplier Material materials with Elongación of 1100 % | ASTM D412 | min. | 500 mm/min |
Módulo a elongación del 300 % | 0.00016 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00016 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 9.9e-05 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 9.9e-05 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 9.8 kN/m Show Supplier Material materials with Resistencia a desgarros of 9.8 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 2.8 MPa Show Supplier Material materials with Resistencia a la tracción of 2.8 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.7 - 2.3 % Show Supplier Material materials with Contracción of 1.7 - 2.3 % | ASTM D955 | Transverse |
1.9 - 2.5 % Show Supplier Material materials with Contracción of 1.9 - 2.5 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 21.6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 21.6 g/10min | ASTM D1238 | 190°C/1.2kg |
Technological properties
Property | ||
---|---|---|
Application areas | Shoes insole, medical appliances | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent | |
Other | Overmolding capabilities: PP |