General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.82 - 0.88 g/cm³ Show Supplier Material materials with Densidad of 0.82 - 0.88 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongación | 1100.6 % Show Supplier Material materials with Elongación of 1100.6 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.0001 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0001 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 6e-05 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 6e-05 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 2.1 kN/m Show Supplier Material materials with Resistencia a desgarros of 2.1 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 0.603 MPa Show Supplier Material materials with Resistencia a la tracción of 0.603 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 2.2 - 2.8 % Show Supplier Material materials with Contracción of 2.2 - 2.8 % | ASTM D955 | Transverse |
3 - 3.6 % Show Supplier Material materials with Contracción of 3 - 3.6 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 353.3 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 353.3 g/10min | ASTM D1238 | 190°C/1.2kg |
Technological properties
Property | ||
---|---|---|
Application areas | Rehabilitation ball, sticker toys, fishing bait, personal care | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent |