General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.89 - 0.95 g/cm³ Show Supplier Material materials with Densidad of 0.89 - 0.95 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 52 - 58 [-] Show Supplier Material materials with Dureza Shore A of 52 - 58 [-] | ASTM D2240 | |
Elongación | 805.7 % Show Supplier Material materials with Elongación of 805.7 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.00125 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00125 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00083 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00083 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 18.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 18.0 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 4.4 MPa Show Supplier Material materials with Resistencia a la tracción of 4.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Contracción of 1.5 - 2.1 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 43.9 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 43.9 g/10min | ASTM D1238 | 190°C/1.2kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hanger clip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PS, HIPS |