General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.01 - 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.01 - 1.07 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 52 - 58 [-] Show Supplier Material materials with Dureza Shore A of 52 - 58 [-] | ASTM D2240 | |
Elongación | 475 % Show Supplier Material materials with Elongación of 475 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.002 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.002 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00132 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00132 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 14.4 kN/m Show Supplier Material materials with Resistencia a desgarros of 14.4 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 2.4 MPa Show Supplier Material materials with Resistencia a la tracción of 2.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.7 - 1.3 % Show Supplier Material materials with Contracción of 0.7 - 1.3 % | ASTM D955 | Transverse |
1 - 1.6 % Show Supplier Material materials with Contracción of 1 - 1.6 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 42.7 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 42.7 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hand tool, kitchenware | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |