General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.92 - 0.98 g/cm³ Show Supplier Material materials with Densidad of 0.92 - 0.98 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 67 - 73 [-] Show Supplier Material materials with Dureza Shore A of 67 - 73 [-] | ASTM D2240 | ||
Elongación | 534.1 % Show Supplier Material materials with Elongación of 534.1 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.0031 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0031 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.00238 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00238 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 24.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 24.0 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 4.0 MPa Show Supplier Material materials with Resistencia a la tracción of 4.0 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 7 °C | 55.4 [-] Show Supplier Material materials with Set de compresión of 55.4 [-] | ||
23 °C | 26.7 [-] Show Supplier Material materials with Set de compresión of 26.7 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.7 - 1.3 % Show Supplier Material materials with Contracción of 0.7 - 1.3 % | ASTM D955 | Transverse |
0.8 - 1.4 % Show Supplier Material materials with Contracción of 0.8 - 1.4 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 30 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 30 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Sports, stationery, toys, tool grip, toothbrush, chopping board | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |