General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.06 - 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.06 - 1.12 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 62 - 68 [-] Show Supplier Material materials with Dureza Shore A of 62 - 68 [-] | ASTM D2240 | |
Elongación | 44.9 % Show Supplier Material materials with Elongación of 44.9 % | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 7.2 kN/m Show Supplier Material materials with Resistencia a desgarros of 7.2 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 1.6 MPa Show Supplier Material materials with Resistencia a la tracción of 1.6 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.6 - 1.2 % Show Supplier Material materials with Contracción of 0.6 - 1.2 % | ASTM D955 | Transverse |
0.9 - 1.5 % Show Supplier Material materials with Contracción of 0.9 - 1.5 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 164.9 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 164.9 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hand tool, car mat | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |