General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.06 - 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.06 - 1.12 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 47 - 53 [-] Show Supplier Material materials with Dureza Shore A of 47 - 53 [-] | ASTM D2240 | ||
Elongación | 412.8 % Show Supplier Material materials with Elongación of 412.8 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.00165 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00165 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.00105 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00105 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 11.1 kN/m Show Supplier Material materials with Resistencia a desgarros of 11.1 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 2.0 MPa Show Supplier Material materials with Resistencia a la tracción of 2.0 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 23 °C | 14.5 [-] Show Supplier Material materials with Set de compresión of 14.5 [-] | ASTM D395 B | |
70 °C | 88.2 [-] Show Supplier Material materials with Set de compresión of 88.2 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.1 - 1.7 % Show Supplier Material materials with Contracción of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 31.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 31.5 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Tool grip, toothbrush, non-slip mat, buttons and knobs, pen grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |