General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.11 - 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.11 - 1.17 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 47 - 53 [-] Show Supplier Material materials with Dureza Shore A of 47 - 53 [-] | ASTM D2240 | ||
Elongación | 575.3 % Show Supplier Material materials with Elongación of 575.3 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.00181 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00181 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.0012 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.0012 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 15.5 kN/m Show Supplier Material materials with Resistencia a desgarros of 15.5 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 2.8 MPa Show Supplier Material materials with Resistencia a la tracción of 2.8 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 23 °C | 15.4 [-] Show Supplier Material materials with Set de compresión of 15.4 [-] | ASTM D395 B | |
70 °C | 88 [-] Show Supplier Material materials with Set de compresión of 88 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.3 - 1.9 % Show Supplier Material materials with Contracción of 1.3 - 1.9 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Contracción of 1.5 - 2.1 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 7.8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 7.8 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Dropper bulb, seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |