General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.94 - 1 g/cm³ Show Supplier Material materials with Densidad of 0.94 - 1 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 77 - 83 [-] Show Supplier Material materials with Dureza Shore A of 77 - 83 [-] | ASTM D2240 | ||
Elongación | 798.8 % Show Supplier Material materials with Elongación of 798.8 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.00413 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00413 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.0029 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.0029 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 42.7 kN/m Show Supplier Material materials with Resistencia a desgarros of 42.7 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 10.3 MPa Show Supplier Material materials with Resistencia a la tracción of 10.3 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 23 °C | 25.3 [-] Show Supplier Material materials with Set de compresión of 25.3 [-] | ASTM D395 B | |
70 °C | 45.9 [-] Show Supplier Material materials with Set de compresión of 45.9 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % | ASTM D955 | |
1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % | ASTM D955 | Transverse | |
Velocidad de flujo de la masa derretida | 1.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 1.5 g/10min | ASTM D1238 | 200°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe seal, valve seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Natural | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |