General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.9 - 0.96 g/cm³ Show Supplier Material materials with Densidad of 0.9 - 0.96 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 87 - 93 [-] Show Supplier Material materials with Dureza Shore A of 87 - 93 [-] | ASTM D2240 | |
Elongación | 856.1 % Show Supplier Material materials with Elongación of 856.1 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.00599 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00599 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00623 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00623 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 68.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 68.0 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 10.4 MPa Show Supplier Material materials with Resistencia a la tracción of 10.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.5 - 1.1 % Show Supplier Material materials with Contracción of 0.5 - 1.1 % | ASTM D955 | Transverse |
0.6 - 1.2 % Show Supplier Material materials with Contracción of 0.6 - 1.2 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 14.2 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 14.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Car carpet | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Natural | |
Other | Overmolding capabilities: PP |