General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.06 - 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.06 - 1.12 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 67 - 73 [-] Show Supplier Material materials with Dureza Shore A of 67 - 73 [-] | ASTM D2240 | |
Elongación | 903.6 % Show Supplier Material materials with Elongación of 903.6 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.00305 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00305 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00219 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00219 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 34.9 kN/m Show Supplier Material materials with Resistencia a desgarros of 34.9 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 6.9 MPa Show Supplier Material materials with Resistencia a la tracción of 6.9 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.4 - 2 % Show Supplier Material materials with Contracción of 1.4 - 2 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Contracción of 1.5 - 2.1 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 3.4 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.4 g/10min | ASTM D1238 | 200°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Tool grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |