General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.97 - 1.03 g/cm³ Show Supplier Material materials with Densidad of 0.97 - 1.03 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 92 - 98 [-] Show Supplier Material materials with Dureza Shore A of 92 - 98 [-] | ASTM D2240 | |
Elongación | 695 % Show Supplier Material materials with Elongación of 695 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.0126 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0126 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.0124 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.0124 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 102.5 kN/m Show Supplier Material materials with Resistencia a desgarros of 102.5 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 17.3 MPa Show Supplier Material materials with Resistencia a la tracción of 17.3 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1 - 1.6 % Show Supplier Material materials with Contracción of 1 - 1.6 % | ASTM D955 | |
1 - 1.6 % Show Supplier Material materials with Contracción of 1 - 1.6 % | ASTM D955 | Transverse | |
Velocidad de flujo de la masa derretida | 13.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 13.5 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive battery sealing | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |