General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Densidad of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 42 - 48 [-] Show Supplier Material materials with Dureza Shore A of 42 - 48 [-] | ASTM D2240 | ||
Elongación | 874.7 % Show Supplier Material materials with Elongación of 874.7 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.0015 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0015 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.00097 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00097 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 14.6 kN/m Show Supplier Material materials with Resistencia a desgarros of 14.6 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 3.7 MPa Show Supplier Material materials with Resistencia a la tracción of 3.7 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 23 °C | 18.5 [-] Show Supplier Material materials with Set de compresión of 18.5 [-] | ASTM D395 B | |
70 °C | 51.2 [-] Show Supplier Material materials with Set de compresión of 51.2 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.4 - 2 % Show Supplier Material materials with Contracción of 1.4 - 2 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Contracción of 1.5 - 2.1 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 34.2 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 34.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, tool grip, toothbrush, pen grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP |