General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Densidad of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 72 - 78 [-] Show Supplier Material materials with Dureza Shore A of 72 - 78 [-] | ASTM D2240 | |
Elongación | 889.6 % Show Supplier Material materials with Elongación of 889.6 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.00358 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00358 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.0026 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.0026 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 38.7 kN/m Show Supplier Material materials with Resistencia a desgarros of 38.7 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 9.2 MPa Show Supplier Material materials with Resistencia a la tracción of 9.2 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % | ASTM D955 | |
1.2 - 1.8 % Show Supplier Material materials with Contracción of 1.2 - 1.8 % | ASTM D955 | Transverse | |
Velocidad de flujo de la masa derretida | 25.2 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 25.2 g/10min | ASTM D1238 | 190°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Face mask, medical appliances, extrusion profiles | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Translucent | |
Other | Overmolding capabilities: PP |