General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.85 - 0.92 g/cm³ Show Supplier Material materials with Densidad of 0.85 - 0.92 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 67 - 73 [-] Show Supplier Material materials with Dureza Shore A of 67 - 73 [-] | ASTM D2240 | ||
Elongación | 755.7 % Show Supplier Material materials with Elongación of 755.7 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.00382 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00382 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.00263 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00263 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 41.2 kN/m Show Supplier Material materials with Resistencia a desgarros of 41.2 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 7.4 MPa Show Supplier Material materials with Resistencia a la tracción of 7.4 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 23 °C | 24.8 [-] Show Supplier Material materials with Set de compresión of 24.8 [-] | ASTM D395 B | |
70 °C | 68.1 [-] Show Supplier Material materials with Set de compresión of 68.1 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.3 - 1.9 % Show Supplier Material materials with Contracción of 1.3 - 1.9 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Contracción of 1.5 - 2.1 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 5.9 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 5.9 g/10min | ASTM D1238 | 190°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubes | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Translucent | |
Other | Overmolding capabilities: PP |