General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Densidad of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 77 - 83 [-] Show Supplier Material materials with Dureza Shore A of 77 - 83 [-] | ASTM D2240 | |
Elongación | 991.3 % Show Supplier Material materials with Elongación of 991.3 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.00552 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00552 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00425 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00425 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 60.7 kN/m Show Supplier Material materials with Resistencia a desgarros of 60.7 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 12.7 MPa Show Supplier Material materials with Resistencia a la tracción of 12.7 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.6 - 1.2 % Show Supplier Material materials with Contracción of 0.6 - 1.2 % | ASTM D955 | Transverse |
0.7 - 1.3 % Show Supplier Material materials with Contracción of 0.7 - 1.3 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 10.1 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10.1 g/10min | ASTM D1238 | 190°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, extrusion profiles, tube and many more… | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Translucent | |
Other | Overmolding capabilities: PP | |
Processing methods |