General
Property | Value | Testing Standard |
---|---|---|
Densidad | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Densidad of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 62 - 68 [-] Show Supplier Material materials with Dureza Shore A of 62 - 68 [-] | ASTM D2240 | ||
Elongación | 795.2 % Show Supplier Material materials with Elongación of 795.2 % | ASTM D412 | 500 mm/min | |
Módulo a elongación del 300 % | 0.00255 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.00255 GPa | ASTM D412 | 500 mm/min | |
Módulo al 100 % de elongación | 0.00172 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00172 GPa | ASTM D412 | 500 mm/min | |
Resistencia a desgarros | 25.9 kN/m Show Supplier Material materials with Resistencia a desgarros of 25.9 kN/m | ASTM D624 Die C | 500 mm/min | |
Resistencia a la tracción | 6.2 MPa Show Supplier Material materials with Resistencia a la tracción of 6.2 MPa | ASTM D412 | 500 mm/min | |
Set de compresión | 23 °C | 29.3 [-] Show Supplier Material materials with Set de compresión of 29.3 [-] | ASTM D395 B | |
70 °C | 54 [-] Show Supplier Material materials with Set de compresión of 54 [-] | ASTM D395 B |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1 - 1.6 % Show Supplier Material materials with Contracción of 1 - 1.6 % | ASTM D955 | |
1 - 1.6 % Show Supplier Material materials with Contracción of 1 - 1.6 % | ASTM D955 | Transverse | |
Velocidad de flujo de la masa derretida | 140 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 140 g/10min | ASTM D1238 | 190°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, container seal, toothbrush grip and many more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP | |
Processing methods |