General
Property | Value | Testing Standard | |
---|---|---|---|
Densidad | 1.14 - 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.14 - 1.2 g/cm³ | ASTM D792 | |
Recycled Content | 30-40 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 42 - 48 [-] Show Supplier Material materials with Dureza Shore A of 42 - 48 [-] | ASTM D2240 | |
Elongación | 831 % Show Supplier Material materials with Elongación of 831 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.0011 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0011 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00077 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00077 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 13.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 13.0 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 2.5 MPa Show Supplier Material materials with Resistencia a la tracción of 2.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.6 - 1.2 % Show Supplier Material materials with Contracción of 0.6 - 1.2 % | ASTM D955 | Transverse |
0.7 - 1.3 % Show Supplier Material materials with Contracción of 0.7 - 1.3 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 16.2 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 16.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | PP Modifier, Grip, Sports and mamy more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Other | Overmolding capabilities: PP | |
Processing methods |