General
Property | Value | Testing Standard | |
---|---|---|---|
Densidad | 1.16 - 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.16 - 1.22 g/cm³ | ASTM D792 | |
Recycled Content | 25-35 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 47 - 53 [-] Show Supplier Material materials with Dureza Shore A of 47 - 53 [-] | ASTM D2240 | |
Elongación | 785.2 % Show Supplier Material materials with Elongación of 785.2 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.0012 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0012 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.00082 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.00082 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 11.3 kN/m Show Supplier Material materials with Resistencia a desgarros of 11.3 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 2.2 MPa Show Supplier Material materials with Resistencia a la tracción of 2.2 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.8 - 1.4 % Show Supplier Material materials with Contracción of 0.8 - 1.4 % | ASTM D955 | Transverse |
1 - 1.6 % Show Supplier Material materials with Contracción of 1 - 1.6 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 23.6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 23.6 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical boot and many more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Processing methods |