General
Property | Value | Testing Standard | |
---|---|---|---|
Densidad | 1.05 - 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.05 - 1.1 g/cm³ | ASTM D792 | |
Recycled Content | 35-45 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore A | 87 - 93 [-] Show Supplier Material materials with Dureza Shore A of 87 - 93 [-] | ASTM D2240 | |
Elongación | 397.3 % Show Supplier Material materials with Elongación of 397.3 % | ASTM D412 | 500 mm/min |
Módulo a elongación del 300 % | 0.0063 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.0063 GPa | ASTM D412 | 500 mm/min |
Módulo al 100 % de elongación | 0.0057 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.0057 GPa | ASTM D412 | 500 mm/min |
Resistencia a desgarros | 45.3 kN/m Show Supplier Material materials with Resistencia a desgarros of 45.3 kN/m | ASTM D624 Die C | 500 mm/min |
Resistencia a la tracción | 6.7 MPa Show Supplier Material materials with Resistencia a la tracción of 6.7 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 1.1 - 1.7 % Show Supplier Material materials with Contracción of 1.1 - 1.7 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Contracción of 1.5 - 2.1 % | ASTM D955 | ||
Velocidad de flujo de la masa derretida | 17.6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17.6 g/10min | ASTM D1238 | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Tool Grip and many more... | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Black | |
Processing methods |