General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 0.88 g/cm³ Show Supplier Material materials with Densidad of 0.88 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 20.0 °C | 25 [-] Show Supplier Material materials with Dureza Shore A of 25 [-] | ASTM D2240 |
Elongación | 20.0 °C | 543 % Show Supplier Material materials with Elongación of 543 % | ASTM D412 |
Módulo al 100 % de elongación | 20.0 °C | 0.74 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.74 GPa | ASTM D412 |
Resistencia a desgarros | 20.0 °C | 9.82 kN/m Show Supplier Material materials with Resistencia a desgarros of 9.82 kN/m | ASTM D624 |
Resistencia a la tracción | 20.0 °C | 2.4 MPa Show Supplier Material materials with Resistencia a la tracción of 2.4 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Elastocon® 2825PE is FDA compliant and well suited for consumer goods and industrial applications requiring UV stability. | |
Other | Elastocon® 2825PE thermoplastic elastomer compound does not require drying. Elastocon® thermoplastic elastomers are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded and coextruded with polyethylene. | |
Processing methods | Injection molding, extrusion, blow molding. |