General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 42 % Show Supplier Material materials with Elongación of 42 % | ASTM D 638 | break |
Módulo de flexión | 23.0 °C | 1 GPa Show Supplier Material materials with Módulo de flexión of 1 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 1.4 GPa Show Supplier Material materials with Módulo elástico of 1.4 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 20 MPa Show Supplier Material materials with Resistencia a la flexión of 20 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 25 MPa Show Supplier Material materials with Resistencia a la tracción of 25 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 26 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 3 % Show Supplier Material materials with Contracción of 3 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |