General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.76 g/cm³ Show Supplier Material materials with Densidad of 1.76 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.78 [-] Show Supplier Material materials with Densidad relativa of 1.78 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 0.3 % Show Supplier Material materials with Elongación of 0.3 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 54 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 54 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 5 J Show Supplier Material materials with Instrumented Impact, Total Energy of 5 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 21.4 GPa Show Supplier Material materials with Módulo de flexión of 21.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 18.4 GPa Show Supplier Material materials with Módulo elástico of 18.4 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 84 MPa Show Supplier Material materials with Resistencia a la flexión of 84 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 54 MPa Show Supplier Material materials with Resistencia a la tracción of 54 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 1 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 1 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 3 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 1.26E-3 J/(kg·K) Show Supplier Material materials with Calor específico of 1.26E-3 J/(kg·K) | ASTM C 351 | ||
Conductividad térmica | 23.0 °C | 15 W/(m·K) Show Supplier Material materials with Conductividad térmica of 15 W/(m·K) | ASTM E 1461-07 | ?25*0.4mm disc | ||
Heat deflection temperature, 0.45 MPa | 275 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 275 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 238 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 238 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de flexión bajo carga | 238 - 275 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 238 - 275 °C | ||||
Thermal conductivity, through-plane | 23.0 °C | 3.5 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 3.5 W/(m·K) | ASTM E 1461-07 | 10*10*3mm sample | ||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101364448- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101069096- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 1.2 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 1.2 kV/mm | IEC 60243-1 | 1.6 mm |
Sheet resistivity, ROA | 23.0 °C | 2.40E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 2.40E+15 Ω | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | IEC 60112 | |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Swimming Pool/Spa, Non-LED Lighting, LED Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |