General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.9 g/cm³ Show Supplier Material materials with Densidad of 1.9 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 0.6 % Show Supplier Material materials with Elongación of 0.6 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 11.2 GPa Show Supplier Material materials with Módulo de flexión of 11.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 12.2 GPa Show Supplier Material materials with Módulo elástico of 12.2 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 47 MPa Show Supplier Material materials with Resistencia a la flexión of 47 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 44 MPa Show Supplier Material materials with Resistencia a la tracción of 44 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 25 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.6E-5 1/K | ASTM E 831 | 40°C to 120°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 5.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 5.1E-5 1/K | ASTM E 831 | 40°C to 120°C |
Conductividad térmica | 23.0 °C | 1.95 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1.95 W/(m·K) | ISO 22007-2 | ?80*3mm discs |
Heat deflection temperature, 1.80 MPa | 191 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 191 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 191 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 191 °C | ||
Thermal conductivity, through-plane | 23.0 °C | 0.9 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 0.9 W/(m·K) | ISO 22007-2 | ?80*3mm discs |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, LED Lighting, Medical Device, Non-LED Lighting, Wireless Communications | |
Availability | Europe,Asia | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |