General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.06 % Show Supplier Material materials with Absorción de agua of 0.06 % | ASTM D 570 | (23°C/24hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 18 % Show Supplier Material materials with Elongación of 18 % | ASTM D 638 | brk, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 111 MPa Show Supplier Material materials with Resistencia a la flexión of 111 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 160 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 160 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 122 - 133 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 122 - 133 °C | ||
Temperatura de reblandecimiento Vicat | 150 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ASTM D 1525 | Rate B/50 | |
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 775°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221212- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.49 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.49 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 2.57 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.57 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 2.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.6E-3 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 5.2E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 5.2E-3 [-] | ASTM D 150 | 50/60 Hz |
Rigidez dieléctrica | 23.0 °C | 18.8 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18.8 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 2.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Electronics, Energy Management, Enclosure/Housing/Cover, Heavy Vehicles, Head Protection, Gas/Electric Oven, Industrial Material Handling, Freezer, Auto Aftermarket, Circuit Protection, Air Conditioning, Dishwasher, Displays, Document Handling, Data Management, Bottles, Coffee Maker/Espresso Machine, Washing Machine, Vacuum Cleaner, Swimming Pool/Spa, Wireless Communications, Personal Care, Non-LED Lighting, Personal Computing, Laundry Dryer, Meter Water, LED Lighting, Photovoltaic Components, Power Manangement, Pump, Refrigerator, Small Appliance, Rail | |
Availability | Europe,Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 245 to 295.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |