NORYL™ Resin PX9406 - Asia

Want to keep this datasheet? Save it now in your required format

Description

Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

0.06 %

Show Supplier Material materials with Absorción de agua of 0.06 %

ASTM D 570 | (23°C/24hrs)

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

9.5 %

Show Supplier Material materials with Elongación of 9.5 %

ASTM D 638 | yld, Type I, 50 mm/min

Módulo de flexión

23.0 °C

2.6 GPa

Show Supplier Material materials with Módulo de flexión of 2.6 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Resistencia a la flexión

23.0 °C

111 MPa

Show Supplier Material materials with Resistencia a la flexión of 111 MPa

ASTM D 790 | yld, 2.6 mm/min, 100 mm span

Resistencia a la tracción

23.0 °C

55 MPa

Show Supplier Material materials with Resistencia a la tracción of 55 MPa

ASTM D 638 | brk, Type I, 50 mm/min

Resistencia al choque, ensayo Izod entallado

23.0 °C

160 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 160 kJ/m²

ASTM D 256 | notched, 23°C

Aplicaciones térmicas

PropertyValueComment

Heat deflection temperature, 0.45 MPa

133 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C

ASTM D 648 | 6.4 mm, unannealed

Heat deflection temperature, 1.80 MPa

122 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C

ASTM D 648 | 6.4 mm, unannealed

Temperatura de flexión bajo carga

122 - 133 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 122 - 133 °C

Temperatura de reblandecimiento Vicat

150 °C

Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 150 °C

ASTM D 1525 | Rate B/50

Inflamabilidad

UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=237097- -

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica, 1 MHz

23.0 °C

2.49 [-]

Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.49 [-]

ASTM D 150

Dielectric constant, 60Hz

23.0 °C

2.57 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.57 [-]

ASTM D 150 | 50/60 Hz

Dissipation factor, 1MHz

23.0 °C

2.6E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 2.6E-3 [-]

ASTM D 150 |

Dissipation factor, 50Hz

23.0 °C

5.2E-3 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 5.2E-3 [-]

ASTM D 150 | 50/60 Hz

Rigidez dieléctrica

23.0 °C

18.8 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 18.8 kV/mm

ASTM D 149 | in oil, 3.2 mm

Sheet resistivity, ROA

23.0 °C

1.00E+16 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω

>, ASTM D 257

Volume resistivity

23.0 °C

2.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.00E+16 Ω·cm

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.5 %

Show Supplier Material materials with Contracción of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Electronic Components, Enclosures, Electronics, Energy Management, Enclosure/Housing/Cover, Heavy Vehicles, Head Protection, Gas/Electric Oven, Industrial Material Handling, Freezer, Auto Aftermarket, Circuit Protection, Air Conditioning, Dishwasher, Displays, Document Handling, Data Management, Bottles, Coffee Maker/Espresso Machine, Washing Machine, Vacuum Cleaner, Swimming Pool/Spa, Wireless Communications, Personal Care, Non-LED Lighting, Personal Computing, Laundry Dryer, Meter Water, LED Lighting, Photovoltaic Components, Power Manangement, Pump, Refrigerator, Small Appliance, Rail

Availability

Europe,Asia,Americas

Processing methods

Mold Temperature: 70 to 100.0°C
Screw Speed: 20 to 100.0rpm
Drying Time: 3 to 4.0hrs
Drying Temperature: 105 to 110.0°C
Nozzle Temperature: 275 to 305.0°C
Rear - Zone 1 Temperature: 245 to 295.0°C
Melt Temperature: 275 to 305.0°C
Vent Depth: 0.038 to 0.051mm
Drying Time (Cumulative): 8hrs
Front - Zone 3 Temperature: 265 to 305.0°C
Back Pressure: 0.3 to 0.7MPa
Middle - Zone 2 Temperature: 255 to 300.0°C
Shot to Cylinder Size: 30 to 70.0%
Maximum Moisture Content: 0.02%

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.