General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 |
Índice límite de óxigeno | 23.0 °C | 38 % Show Supplier Material materials with Índice límite de óxigeno of 38 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5.2 % Show Supplier Material materials with Elongación of 5.2 % | ISO 527 | yield, 50 mm/min |
Hardness, Rockwell L | 23.0 °C | 84 [-] Show Supplier Material materials with Hardness, Rockwell L of 84 [-] | ASTM D 785 |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Supplier Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 700 J/m | ASTM D 256 | -40°C |
Instrumented Impact, Total Energy | 23.0 °C | 66 J Show Supplier Material materials with Instrumented Impact, Total Energy of 66 J | ASTM D 3763 | -30°C |
Módulo de flexión | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo de flexión of 2.1 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 84 MPa Show Supplier Material materials with Resistencia a la flexión of 84 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 54 MPa Show Supplier Material materials with Resistencia a la tracción of 54 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 69 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 73 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 73 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 9.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 9.8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature, 0.45 MPa | 119 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 119 °C | ISO 75/Cf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 108 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 108 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 108 - 119 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 108 - 119 °C | ||||
Temperatura de reblandecimiento Vicat | 124 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 124 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥3.0mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104423704- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.81 [-] Show Supplier Material materials with Constante dieléctrica of 2.81 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 10GHz | 23.0 °C | 2.84 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 2.84 [-] | SABIC method |
Dielectric constant, 1GHz | 23.0 °C | 2.87 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.87 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 2.81 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 2.81 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 6.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6.4E-3 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 6E-3 [-] | SABIC method |
Factor de disipación | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Factor de disipación of 6E-3 [-] | SABIC method |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción transversal of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 12 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 12 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 11 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 11 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction Sheet, Data Management, Data Transfer, Displays, Document Handling, Aerospace, Air Conditioning, Audio, Lawn/Garden, Heavy Vehicles, Freezer, Engine Cooling System, EV Infrastructure, Electronics, Energy Management, Enclosure/Housing/Cover, Enclosures, Electronic Components, Non-LED Lighting, Personal Computing, LED Lighting, Infrastructure, Small Appliance, Security/Detection, Respiratory, Photo/Video Camera, Vacuum Cleaner, Swimming Pool/Spa, Wiring Devices, Watch/Jewelry, Wearables, Wireless Communications, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |