General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.26 [-] Show Supplier Material materials with Densidad relativa of 1.26 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.6 % Show Supplier Material materials with Elongación of 6.6 % | SABIC - Japan Method | brk, Type I, 10 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 66.4 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 66.4 J/m | ASTM D 256 | notched, 23°C |
Módulo de flexión | 23.0 °C | 9.7 GPa Show Supplier Material materials with Módulo de flexión of 9.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 155 MPa Show Supplier Material materials with Resistencia a la flexión of 155 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 120.7 MPa Show Supplier Material materials with Resistencia a la tracción of 120.7 MPa | SABIC - Japan Method | yld, Type I, 10 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 66.4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 66.4 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 17.82 % Show Supplier Material materials with Contenido de cenizas of 17.82 % | w/w | ||
Heat deflection temperature, 1.80 MPa | 133.4 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133.4 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Temperatura de flexión bajo carga | 133.4 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 133.4 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=237042- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥3mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 42000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 42000 Ω | ASTM D 257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 10.6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10.6 g/10min | ASTM D 1238 | 300°C/5.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical Components & Infrastructure | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |