General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.08 % Show Supplier Material materials with Absorción de agua of 0.08 % | ASTM D 570 | (23°C/24hrs) |
Densidad relativa | 23.0 °C | 1.13 [-] Show Supplier Material materials with Densidad relativa of 1.13 [-] | ASTM D 792 | |
Índice límite de óxigeno | 23.0 °C | 39 % Show Supplier Material materials with Índice límite de óxigeno of 39 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 9.2 % Show Supplier Material materials with Elongación of 9.2 % | ISO 527 | break, 50 mm/min |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 293 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 293 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 100 J/m | ASTM D 4812 | unnotched, -30°C |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 87 MPa Show Supplier Material materials with Resistencia a la flexión of 87 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | ISO 527 | break, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | ISO 179/2C | 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 20 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 76 mg/1000cy Show Supplier Material materials with Taber Abrasion of 76 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Conductividad térmica | 23.0 °C | 0.24 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.24 W/(m·K) | ASTM C177 | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 95 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 95 °C Show Supplier Material materials with Relative temperature index, electrical of 95 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 95 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C | UL 746B | |||
Temperatura de flexión bajo carga | 82 - 95 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 82 - 95 °C | ||||
Temperatura de reblandecimiento Vicat | 107 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 107 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100110158- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100110159- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 100 Hz | 23.0 °C | 2.74 [-] Show Supplier Material materials with Constante dieléctrica, 100 Hz of 2.74 [-] | ASTM D 150 |
Dielectric constant, 1KHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 1KHz of 2.6 [-] | ASTM D 150 |
Dissipation factor, 100Hz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 0.01 [-] | ASTM D 150 |
Dissipation factor, 100kHz | 23.0 °C | 5.5E-3 [-] Show Supplier Material materials with Dissipation factor, 100kHz of 5.5E-3 [-] | ASTM D 150 |
High Amp Arc Ignition | 23.0 °C | 6 mm Show Supplier Material materials with High Amp Arc Ignition of 6 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 6 mm Show Supplier Material materials with Hot-Wire Ignition of 6 mm | ≥, UL 746A | PLC 1 |
Rigidez dieléctrica | 23.0 °C | 19.2 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 19.2 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Volume resistivity | 23.0 °C | 1.80E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.80E+16 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 1 V Show Supplier Material materials with Índice de seguimiento comparativo of 1 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 20 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 20 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 23 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Vending Machine, Swimming Pool/Spa, Wireless Communications, Wiring Devices, Wearables, Laser Sintering, Power Manangement, Photovoltaic Components, Plumbing, Photo/Video Camera, Servingware, Small Appliance, Surgical Devices, Security/Detection, Respiratory, Monitoring and Imaging, Meter Water, Medical Facility Infrastructure, LED Lighting, Medical Device, Personal Computing, Personal Care, Non-LED Lighting, Document Handling, Door Handle, Displays, Data Transfer, Data Management, Algae, Building Element, Circuit Protection, Audio, Air Conditioning, Electronic Components, Enclosures, Energy Management, Electronics, Enclosure/Housing/Cover, Lab Ware and Clinical Diagnostics, Heavy Vehicles, Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Nozzle Temperature: 250 to 275.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |