General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.25 % Show Supplier Material materials with Absorción de agua of 0.25 % | ASTM D 570 | (23°C/24hrs) |
Densidad | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Densidad of 1.31 g/cm³ | ISO 1183 | (Molded) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 32 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 8.4 GPa Show Supplier Material materials with Módulo de flexión of 8.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 9 GPa Show Supplier Material materials with Módulo elástico of 9 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 225 MPa Show Supplier Material materials with Resistencia a la flexión of 225 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 156 MPa Show Supplier Material materials with Resistencia a la tracción of 156 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | ISO 179/1eA | 80*10*4mm, Cut, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.56E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.56E-5 1/K | ASTM E 831 | 40°C to 120°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.25E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6.25E-5 1/K | ASTM E 831 | 40°C to 120°C | ||
Heat deflection temperature, 1.80 MPa | 201 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 201 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Temperatura de flexión bajo carga | 201 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 201 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101997197- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.4mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 397000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 397000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 508000 Ω·cm Show Supplier Material materials with Volume resistivity of 508000 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción transversal of 0.5 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 31 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 31 g/10min | ASTM D 1238 | 367°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |