General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.351 g/cm³ Show Supplier Material materials with Densidad of 1.351 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 48 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 48 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 354 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 354 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 11.6 GPa Show Supplier Material materials with Módulo de flexión of 11.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 17 GPa Show Supplier Material materials with Módulo elástico of 17 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 233 MPa Show Supplier Material materials with Resistencia a la flexión of 233 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 224 MPa Show Supplier Material materials with Resistencia a la tracción of 224 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 48 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 48 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 5000 - 500000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 5000 - 500000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 5.00E+3 - 5.00E+6 Ω·cm Show Supplier Material materials with Volume resistivity of 5.00E+3 - 5.00E+6 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Commercial Appliance | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |