General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 1.99 % Show Supplier Material materials with Absorción de agua of 1.99 % | ISO 62-1 | (23°C/24hrs) |
Densidad relativa | 23.0 °C | 1.1 [-] Show Supplier Material materials with Densidad relativa of 1.1 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.39 % Show Supplier Material materials with Moisture absorption of 0.39 % | ISO 62-4 | (23°C/50% RH/Equilibrium) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 51 % Show Supplier Material materials with Elongación of 51 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D 256 |
Instrumented Impact, at Peak | 23.0 °C | 48 J Show Supplier Material materials with Instrumented Impact, at Peak of 48 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 98 MPa Show Supplier Material materials with Resistencia a la flexión of 98 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 66 MPa Show Supplier Material materials with Resistencia a la tracción of 66 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/2C | -20°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/4A | notched 63.5*12.7*3.2, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9E-5 1/K | ASTM E 831 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.53E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 1.53E-4 1/K | ASTM E 831 | 60°C to 138°C |
Heat deflection temperature, 0.45 MPa | 181 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 181 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Temperatura de flexión bajo carga | 181 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 181 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1MHz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-] | ASTM D 150 |
Rigidez dieléctrica | 23.0 °C | 22.4 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 22.4 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.4 % Show Supplier Material materials with Contracción of 1.4 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 1.2 % Show Supplier Material materials with Contracción transversal of 1.2 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | ASTM D 1238 | 280°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Electrical, Circuit Protection, Auto Aftermarket, Electronic Components, Recreational Vehicle | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 95 to 105.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |