General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.39 [-] Show Supplier Material materials with Densidad relativa of 1.39 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.8 % Show Supplier Material materials with Elongación of 1.8 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 761 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 761 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 23.3 GPa Show Supplier Material materials with Módulo de flexión of 23.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 28.7 GPa Show Supplier Material materials with Módulo elástico of 28.7 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la compresión | 23.0 °C | 234 MPa Show Supplier Material materials with Resistencia a la compresión of 234 MPa | SABIC method |
Resistencia a la flexión | 23.0 °C | 367 MPa Show Supplier Material materials with Resistencia a la flexión of 367 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 265 MPa Show Supplier Material materials with Resistencia a la tracción of 265 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 90 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción transversal of 0.1 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 10 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10 g/10min | ASTM D 1238 | 380°C/6.7 kgf |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |