General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.1 % Show Supplier Material materials with Elongación of 1.1 % | ISO 527 | break |
Módulo de flexión | 23.0 °C | 15.9 GPa Show Supplier Material materials with Módulo de flexión of 15.9 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 20.2 GPa Show Supplier Material materials with Módulo elástico of 20.2 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 269 MPa Show Supplier Material materials with Resistencia a la flexión of 269 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 219 MPa Show Supplier Material materials with Resistencia a la tracción of 219 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 26 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 217 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 217 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Temperatura de flexión bajo carga | 217 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 217 °C | ||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: 0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282614- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft Exteriors, Air Cabin Interiors | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |