General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.4 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.4 [-] | ASTM E 132 |
Elongación | 23.0 °C | 2.4 % Show Supplier Material materials with Elongación of 2.4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 524 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 524 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 9.7 GPa Show Supplier Material materials with Módulo de flexión of 9.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 11.2 GPa Show Supplier Material materials with Módulo elástico of 11.2 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 268 MPa Show Supplier Material materials with Resistencia a la flexión of 268 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 197 MPa Show Supplier Material materials with Resistencia a la tracción of 197 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100000 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |