General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 1.25 % Show Supplier Material materials with Absorción de agua of 1.25 % | ASTM D 570 | (23°C/Saturated) |
Densidad relativa | 23.0 °C | 1.27 [-] Show Supplier Material materials with Densidad relativa of 1.27 [-] | ASTM D 792 | |
Índice límite de óxigeno | 23.0 °C | 44 % Show Supplier Material materials with Índice límite de óxigeno of 44 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell M | 23.0 °C | 109 [-] Show Supplier Material materials with Dureza Rockwell M of 109 [-] | ASTM D 785 | |
Elongación | 23.0 °C | 7 % Show Supplier Material materials with Elongación of 7 % | ASTM D 638 | yld, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 32 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1335 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1335 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 3.5 GPa Show Supplier Material materials with Módulo de flexión of 3.5 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 3.6 GPa Show Supplier Material materials with Módulo elástico of 3.6 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 165 MPa Show Supplier Material materials with Resistencia a la flexión of 165 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.58E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.58E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Conductividad térmica | 23.0 °C | 0.22 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.22 W/(m·K) | ASTM C177 | ||
Heat deflection temperature, 0.45 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 207 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 198 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 198 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Temperatura de flexión bajo carga | 198 - 207 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 198 - 207 °C | ||||
Temperatura de reblandecimiento Vicat | 218 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 218 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | NBS Smoke Density, Flaming, Ds 4 min: 2- ASTM E 662 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 1.3E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 1.3E-3 [-] | ASTM D 150 |
Factor de disipación | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Factor de disipación of 2.5E-3 [-] | ASTM D 150 | 2450 MHz |
Rigidez dieléctrica | 23.0 °C | 32.6 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 32.6 kV/mm | ASTM D 149 | in air, 1.6 mm |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 17.8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17.8 g/10min | ASTM D 1238 | 337°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Industrial Material Handling, Electronic Material Handling, Semiconductor, Tray | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |