General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | ASTM D 638 | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 192 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 192 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 967 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 967 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 8.4 GPa Show Supplier Material materials with Módulo de flexión of 8.4 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 8.3 GPa Show Supplier Material materials with Módulo elástico of 8.3 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 199 MPa Show Supplier Material materials with Resistencia a la flexión of 199 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 126 MPa Show Supplier Material materials with Resistencia a la tracción of 126 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 192 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 192 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Heavy Vehicles, Food Transportation, Medical Device | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |