General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Densidad of 1.31 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Impact strength, Izod unnotched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 550 J/m | ASTM D 4812 | 23°C | ||
Elongación | ISO 527 | yield, 5 mm/min | ||||
Módulo de flexión | ISO 178 | 2 mm/min | ||||
Módulo elástico | ISO 527 | 1 mm/min | ||||
Resistencia a la flexión | ISO 178 | yield, 2 mm/min | ||||
Resistencia a la tracción | ISO 527 | break, 5 mm/min |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 150 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 150 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 55 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 55 °C | ASTM D 648 | 3.2mm, unannealed |
Temperatura de flexión bajo carga | 55 - 150 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 55 - 150 °C | |
Temperatura de reblandecimiento Vicat | 207 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 207 °C | ASTM D 1525 | Rate A/120 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.8 % Show Supplier Material materials with Contracción of 1.8 % | SABIC method | on tensile bar |
Velocidad de flujo del volumen derretido | 20 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 20 cm³/10min | ISO 1133 | MVR at 250°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive , Electronics | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |