General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua of 0.3 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.19 [-] Show Supplier Material materials with Densidad relativa of 1.19 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 100 % Show Supplier Material materials with Elongación of 100 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 900 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 900 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 72 J Show Supplier Material materials with Instrumented Impact, Total Energy of 72 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 60 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature, 0.45 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 125 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 115 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Temperatura de flexión bajo carga | 115 - 125 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 115 - 125 °C | ||
Temperatura de reblandecimiento Vicat | 135 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 135 °C | ISO 306 | Rate B/120 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 26.5 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26.5 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 | |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 7 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 7 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Velocidad de flujo del volumen derretido | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning, Circuit Protection, Audio, Coffee Maker/Espresso Machine, Data Transfer, Data Management, Dishwasher, Displays, Document Handling, Gas/Electric Oven, Heavy Vehicles, EV Infrastructure, Electronic Components, Enclosures, Enclosure/Housing/Cover, Energy Management, LED Lighting, Medical Device, Meter Gas, Microwave Oven, Monitoring and Imaging, Personal Computing, OLED, Small Appliance, Security/Detection, Power Boat, Power Manangement, Photo/Video Camera, Pharmaceutical Packaging & Drug Delivery, Washing Machine, Wireless Communications, Wiring Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |