General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.49 g/cm³ Show Supplier Material materials with Densidad of 1.49 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 0.7 % Show Supplier Material materials with Elongación of 0.7 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 37 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 37 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 480 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 480 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 30.3 GPa Show Supplier Material materials with Módulo de flexión of 30.3 GPa | ISO 178 | 2 mm/min |
Resistencia a la flexión | 23.0 °C | 290 MPa Show Supplier Material materials with Resistencia a la flexión of 290 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la tracción of 179 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 25 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102581048- - <br> UL Recognized, 94V-0 Flame Class Rating: 1mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |