General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.8 % Show Supplier Material materials with Elongación of 3.8 % | ISO 527 | yield |
Impact strength, Izod notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D 256 | -40°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1790 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1790 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 80 MPa Show Supplier Material materials with Resistencia a la flexión of 80 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | ISO 527 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 14 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 85 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.6E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6.7E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Temperatura de flexión bajo carga | 125 - 136 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 125 - 136 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Shielding effectiveness | 23.0 °C | 40 dB Show Supplier Material materials with Shielding effectiveness of 40 dB | SABIC method | @ 3mm |
Volume resistivity | 23.0 °C | 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Monitoring and Imaging, Personal Computing, Air Cabin Interiors, Document Handling, Cooking Range, Data Transfer, Electronic Components, Electronics, Enclosure/Housing/Cover, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Screw Speed: 30 to 60.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |